THINKY Datasheet
CNF (Carbon Nano Fiber )
Process - Dispersion, Defoaming
Parameter - 2000rpm, 6min
[ Materials ] CNF into eposy
Diameter = 100nm, Length = 10mico
[ Capacity ] 60g (1wt%)
[ Viscosity ] 10,000cP (Estimated)
[ THINKY Mixer ] Vacuum mixer ARV-310