Find how the THINKY mixers improves the mixing quality and reduce processing cycle time.

 

NO time to view each of datasheet?    

    >> Ask us to email you all datasheets

 

Cannot find the similar applications with yours? 

How to find the similarity with your application.
   1. Refer to particle size, length, figure ==> micron or nano size. Fiber, sphere or flake.
   2. Find loading amount ==> high or low loading
   3. Check densities or viscosities. ==> high or low density and/or viscosity
   4. Categorize the materials ==> Polymer, monome, resin, water. 
 
 

Applications

     THINKY  Mixer    

VIscosity, Density,

Particle Volume or Size

Datasheet

1

Ceramic

(10 V%)

Dispersion

Defoaming

ARE-250 

2 minutes

Barium Titanate - 6.02 g/cm3  

Micron particle, 10 volume %,

 (Total 120g)

 2

Nano Ceramic

(70 V%)

Dispersion

Defoaming

ARE-250

3 minutes

Aluminum oxide - 0.5 μm

Nano particle, 3.97g/cm3

50 ~ 70 volume %

View
3 2 part Epoxy

Mixing

Defoaming

 ARE-250

20 seconds

Epoxy

 Part A : 3000-6000 poise

 Part B : 0.3-0.7 poise

View

4Carbon Nano Fiber (10 V%)

Dispersion

ARE-250

3 minutes

CNF - 10 volume %

Nano particle, Fiber

View
5

Carbon Black

2 part silicone

(20 wt%)

Dispersion

Defoaming

ARV-310 1 minutes

/ ARE-250 8 minutes

Nano Carbon Black 20 wt % (50V%)

Nano particle

 (Total 120g)

View
6

Silicone

Potting

Compounds

Mixing

Defoaming

ARV-310

3 minutes

Part A : 4000-8000 poise

Part B : 200-700 poise

 (Total 10g)

View
7 Precious metal paste

Dispersion

Defoaming

 ARV-310

/ ARE-250

from 30 sec.to 1 min

 General silver filled condudctive epoxy / Jar and syringe application

Highly dense metal powder

View

8

Carbon Nano

Tube (1-2 wt%)

Dispersion ARV-310 6 min

 CNT - 1 to 2 wt %

 Nano particle tube

View

9

Zinc Oxide

(10 V%)

Dispersion

Defoaming

 ARE-250 6 min

ZnO 10 volume %

petroleum Jelly 0.85, Zinc Oxide 5.76

View

10

LCD ODF sealant

(10 V%)

Dispersion

Deforming

ARV-5000TWIN

Au Ball 10 volume %

sealant 400,000cP, Au ball 3micron

View

11 Printing InkDegas ARV-5000 Solvent Ink 450g

View

12 Viscous EpoxyDefoaming

ARE-250

 250AD-EFD-3x6

Epoxy 828 2.5cc in EFD 3cc Syringe

View

13 AluminaDispersion

Defoaming

 ARV-5000Aluminum oxide - 20 volume %

Silicone 3000cP 

 View

14 LED PhosphorDispersion

Defoaming

ARV-310

+ Syringe Loader

Phosphor 10 wt %

Slicone 10,000cP  20g

View

15

Viscous EpoxyDefoaming

 ARV-310

+ Syringe Loader

 Various Epoxy sample

View

 16Talc

Dispersion

Defoaming 

 ARE-250

 Silicone 60g - 30wt%

Silicone 10,000cP

 View

17

 CNF (1%wt)Dispersion

Defoaming 

 ARV-310  6min

 CNF 1%wt

 View

 18

Suspension

Particle

Reduction

 ARE-250 3minPhenytoin as API

 View

 

 
* All THINKY mixers are NOT explosion proof.
              - Flammable solvents can be used ONLY with THINKY instructions.
              - Explosive materials can be used ONLY if you have own facilities or tools, with which you can prove your safety. 
 
* Interested in the other mixing samples? >> Visit THINKY JAPAN website